Hi guys,
So I was balancing my 20s 2p 82V LIPO pack the other day going through each of the 10 individual Lipo batteries with balancer 1 by 1. I stupidly lost concentration and ended up with 4 separate balance connectors unplugged.
All of the balance connectors are hooked up to a parallel port for monitoring...
Long story short, I short-circuited two of the balance connectors. I don't think I damaged the batteries themselves, but I did melt a male and female JST-XH connector - see images.
So I'm wondering what the best solution is? Do I cut off the melted connectors and hand solder on replacements? Or do I need a crimper? Or should I buy a pre-crimped/soldered lead and just solder the new leads to the old ones?
Any help would be greatly appreciated!
Thanks guys,
Liam
![Screen Shot 2014-04-06 at 13.38.11.png Screen Shot 2014-04-06 at 13.38.11.png](https://endless-sphere.com/sphere/data/attachments/72/72941-dbede12d869937229daa35ca600b1b0d.jpg)
![Screen Shot 2014-04-06 at 13.36.15.png Screen Shot 2014-04-06 at 13.36.15.png](https://endless-sphere.com/sphere/data/attachments/72/72942-1143893e35c46c7f70177212f31a5290.jpg)
http://www.ebay.co.uk/itm/2x-JST-XH-connector-plug-Male-Female-Crimps-Lipo-4s-Balance-Extension-/230777448177?pt=UK_ToysGames_RadioControlled_JN&hash=item35bb6866f1
http://www.ebay.co.uk/itm/Lipo-Balance-Lead-repairing-battery-pack-4s-JST-XH-male-4-cell-14-8V-22AWG-/231134459655?pt=UK_ToysGames_RadioControlled_JN&hash=item35d0aff707
So I was balancing my 20s 2p 82V LIPO pack the other day going through each of the 10 individual Lipo batteries with balancer 1 by 1. I stupidly lost concentration and ended up with 4 separate balance connectors unplugged.
All of the balance connectors are hooked up to a parallel port for monitoring...
Long story short, I short-circuited two of the balance connectors. I don't think I damaged the batteries themselves, but I did melt a male and female JST-XH connector - see images.
So I'm wondering what the best solution is? Do I cut off the melted connectors and hand solder on replacements? Or do I need a crimper? Or should I buy a pre-crimped/soldered lead and just solder the new leads to the old ones?
Any help would be greatly appreciated!
Thanks guys,
Liam
![Screen Shot 2014-04-06 at 13.38.11.png Screen Shot 2014-04-06 at 13.38.11.png](https://endless-sphere.com/sphere/data/attachments/72/72941-dbede12d869937229daa35ca600b1b0d.jpg)
![Screen Shot 2014-04-06 at 13.36.15.png Screen Shot 2014-04-06 at 13.36.15.png](https://endless-sphere.com/sphere/data/attachments/72/72942-1143893e35c46c7f70177212f31a5290.jpg)
http://www.ebay.co.uk/itm/2x-JST-XH-connector-plug-Male-Female-Crimps-Lipo-4s-Balance-Extension-/230777448177?pt=UK_ToysGames_RadioControlled_JN&hash=item35bb6866f1
http://www.ebay.co.uk/itm/Lipo-Balance-Lead-repairing-battery-pack-4s-JST-XH-male-4-cell-14-8V-22AWG-/231134459655?pt=UK_ToysGames_RadioControlled_JN&hash=item35d0aff707