doubledipsoon
100 W
- Joined
- Feb 22, 2013
- Messages
- 151
48V 13Ah lithium ion Bottle ebike battery pack with charger
1. Rated capacity: 13AH
2. Voltage: 48V
3. Charging Voltage: 54.6V
4. Discharge cutoff voltage: 36.4V
5. Cell: 18650 (13S5P) ISR18650-2600mAh(LiMn2O4) This battery pack include 65pcs 18650 cells
6. Standard charging: 0.2C constant current(CC) charge to 54.6V, then constant voltage (CC) 54.6V charge till charge current decline to ≤0.05C
Cycle life:Discharge capacity (500st cycles) ≥60 %( Min Capacity)
7. Continuous discharge current: 30A
8. Pulse/Max discharge current 70A
9. Max charging current : 5A
10. Charging temperature: 0~45℃
11. Dischargeing temperature: -20~55℃,batery management system to prevent overheating
12.Operating voltage:36.4V~54.6V
13. Diamesion: 91x435mm(diameter X heigh)
14.Weight of battery pack:About4.25 kg
1. Rated capacity: 13AH
2. Voltage: 48V
3. Charging Voltage: 54.6V
4. Discharge cutoff voltage: 36.4V
5. Cell: 18650 (13S5P) ISR18650-2600mAh(LiMn2O4) This battery pack include 65pcs 18650 cells
6. Standard charging: 0.2C constant current(CC) charge to 54.6V, then constant voltage (CC) 54.6V charge till charge current decline to ≤0.05C
Cycle life:Discharge capacity (500st cycles) ≥60 %( Min Capacity)
7. Continuous discharge current: 30A
8. Pulse/Max discharge current 70A
9. Max charging current : 5A
10. Charging temperature: 0~45℃
11. Dischargeing temperature: -20~55℃,batery management system to prevent overheating
12.Operating voltage:36.4V~54.6V
13. Diamesion: 91x435mm(diameter X heigh)
14.Weight of battery pack:About4.25 kg