• Howdy! we're looking for donations to finish custom knowledgebase software for this forum. Please see our Funding drive thread

Would this way of sandwich bonding work. Nickel to copper.

Joined
Sep 28, 2023
Messages
62
Location
Long Beach, CA
I've mashed .25 copper to .2 nickel with a pair of heated tip pliers. It has much more surface area than spot welding. It's not super srong but it's a solid connection and quite strong. I sanded both the copper and nickel. The best part is is that it's very flat.

See the shots and tell me what you think.
first shot: sticking a folded in two solder
second: heated pliers melting solder
third: pulling off and seeing that large surface area is good.

Good idea? And better way to have it stick better?
 

Attachments

  • Screenshot 2023-09-28 at 1.26.23 AM.png
    Screenshot 2023-09-28 at 1.26.23 AM.png
    1.1 MB · Views: 23
  • Screenshot 2023-09-28 at 1.26.33 AM.png
    Screenshot 2023-09-28 at 1.26.33 AM.png
    938.4 KB · Views: 23
  • Screenshot 2023-09-28 at 1.27.06 AM.png
    Screenshot 2023-09-28 at 1.27.06 AM.png
    1 MB · Views: 23
I think it would wok, buti believe this method misses some of the benefits of the copper/nickel sandwich.

The shell of the 18650 cell is nickel-plated steel...one of the goas of using a copper/nickel sandwich is to have a weld where the bus copper is directly touching the cell-tips, instead of adding additional sections of nickel to the current-path.

The nickel cap will not be carrying any current. It is only there to produce a hot-spot. Between the nickel above and the steel shell below, the two hot spots will heat the copper just enough to form a weld.
 
well, now you're talking about a real sandwich. thank you for straighten me out. so I'll try my welder out to see if it'll do the copper nickel weld. I hope it does.
should i do anything extra to the copper or nickel? I see some have the nickel/copper cap area pushed in about 1/16" i suppose to raise the rest of the sheet.
 
Back
Top