right heres the settings i have,this is for a normal lithium ion-colbalt pack not fifepo4,my settings in brackets as currently set
1.overvoltage(4.2)
2.overvoltage rlease (4.199)
3.undervoltage (2.75)
4.undervoltage release (2.85)
5. discharge current (50)
6.cycle capacity (16ah)
7.nominal capacity (15.3)
8. charging duration (100)
9.open balace (close)*
10. balance mode (charge balance)
11.balance turn on (3.7v)*
12.balance precision (0.03v)
13. advanced protection parameters ,hardware over current (390.00A)
14. hardware short circuit (665.00A)
its mostly the ones with the asterix at the end that im unsure about that i need explaining,cheers m3vuv.
at the moment the small ballance symbol isnt comming on next to the battery groups,the cell group voltages are
1=4.110v
2. 4.128v
3.4.108v
4. 4.085v
5.4.117v
6. 4.085v
7. 4.099v
8.4.105v
9.4.121v
10.4.118v
11.4.131v
12.4.117v
13.4.119v
do any of these settings need tweaking,as far as i know the pack is about 17ah but put 15,thought that would give me a better warning when it was nealy flat,ie discharger.