Adam271226 said:Hi CiDi,
You mentioned using 43v M500 firmware in M600 motor.
Are there any complications with battery voltage and battery level % after update?
Have you noticed any other differences? (for better or worse?)
Thanks,
With the 43V firmware the current is set at 20A instead of 18A, this means more power but also more overheating and battery consumption.
Level 1 is already high and level 3 is already at full power.
The percentage marked on the display remains at 99% up to approximately 75% of battery consumption.
The disconnection of the discharged battery, the BMS does and not the controller, so you can use the lower voltage battery, over time, battery life may be affected.
Occasionally with fully charged battery the overvoltage error occurs.
I used this 43V firmware because the original 48V was unusable due to jerky operation.
Now with the new 48V firmware it seems that the problem is solved.